Property item | Test condition | Test method | Test data | Data unit |
MFR | GB/T 3682-2000 | 26 | g/10min | |
IZOD impact Strength | -20°C | GB/T 1843-1996 | 4.7 | Kj/m2 |
Rockwell Hardness | GB/T 9342-1988 | 100 | R | |
Flexural Modulus | GB/T 9341-2000 | 1310 | MPa | |
Tensile yield Stress | GB/T 1040.2-2006 | 25.5 | MPa | |
IZOD impact Strength | 23°C | GB/T 1843-1996 | 12 | Kj/m2 |
Load thermal Deformation temperature | GB/T 1634.2-2004 | 95 | °C |