Project | Test data | Data unit | |
Basic properties | Density | 0.921 | g/cm3 |
Melt flow rate | 0.3 | g/10min | |
Mechanical properties | Elongation at break | ≥450 | % |
Tensile strength at break | ≥13 | Mpa |
Performance | Test conditions [state] | Test method | Test data | Data unit | ||
Basic properties | Density | ISO 1183 | 0.925 | g/cm3 | ||
Melt flow rate | 2.16kg | ISO 1133 | 4 | g/10min | ||
Mechanical properties | Elongation | lengthways | ISO 527 | 550 | % | |
crosswise | ISO 527 | 700 | % | |||
Tensile strength | lengthways | ISO 527 | 19 | MPa | ||
crosswise | ISO 527 | 18 | MPa | |||
Tensile strength | ISO 527 | 11 | MPa | |||
Modulus of Elasticity | ISO 527 | 280 | MPa | |||
Shore hardness | ISO 868 | 48 | ||||
Fall out of strength | ASTM D-1709 | 100 | g | |||
Thermal properties |
Vicat softening point | A/50 | ISO 306 | 94 | ºC | |
Melting point | ISO 11357 | 112 | ºC |
Project | Test data | Data unit | |
Basic properties | Density | 0.9205~0.9245 | g/cm3 |
Melt flow rate | 1.7-2.3 | g/10min | |
Mechanical properties | Elongation at break | ≥200 | % |
Tensile strength at break | ≥17 | Mpa | |
Tensile strength yield | ≥3.0 | ||
Shore hardness | ≥44 | ||
Thermal properties |
Vicat softening point | ≥90 | ºC |
Project |
Test method |
Test Data |
Data Unit |
||
MFR(190ºC,2.16ºC) |
2 |
g/10min |
|||
Density |
0.918 |
g/cm³ |
|||
Yield tensile strength |
MD |
12 |
Mpa |
||
TD | 10 | ||||
Tensile strength at break |
MD |
35 |
MPa |
||
TD |
29 |
||||
Elongation at break |
MD |
700 |
% |
||
TD | 750 | ||||
Secant modulus |
MD1% |
220 |
Mpa |
||
TD1% | 260 | ||||
Haze |
13 |
% |
|||
Elmandorf tear strength | MD | 130 | g |
||
TD | 320 | ||||
Vicat softening point | 98 | ºC | |||
Glossiness | 80 |