Customization: | Available |
---|---|
CAS No.: | 9003-53-6 |
Formula: | (C8h8)N |
Still deciding? Get samples of US$ 1/delivery cost to be discussed
Request Sample
|
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
Performance | Test conditions [state] | Test Method | Test data | Data unit |
Melt flow rate | ISO1133/1997 | 4-4.8 | g/10min | |
Density | ISO1183/1987 | 1.030 | g/cm3 | |
Tensile break strength | ISO527-2/1993 | 25 | Mpa | |
Impact strength | ISO180/1993 | 1150 | J/M | |
Vicat softening point | ISO 306/1994 | 90 | ºC | |
Brittle temperature | ISO75-2/1993 | 80 | ºC |
Performance | Test Method | Test data | Data unit |
Melt flow rate | ASTM D-1238 | 4.0 | g/10min |
Density | ASTM D-792 | 1.04 | g/cm3 |
Elongation at break | ASTM D-683 | 30 | % |
TYS | ASTM D-683 | 36.2 | Mpa |
Vicat softening point | ASTM D-1525 | 98 | ºC |
Flexural Modulus | ASTM D-790 | 2060 | Mpa |
Performance | Test data | Data unit |
Melt flow rate | 6-9 | g/10min |
Izodnotched impact strength | 9.6 | Kg-cm/cm |
residual monomers | 700 | ppm |
strength of extension | 195 | Kg/m2 |
Vicat softening point | 92 | ºC |
gloss | 60 |
Performance | Test Method | Test data | Data unit |
Melt flow rate |
ASTM D-1238 |
3.0-4.5 |
g/10min |
Density |
ASTM D-792 |
1.04 |
g/cm3 |
Elongation at break |
ASTM D-683 |
50 |
% |
TYS |
ASTM D-683 |
28 |
Mpa |
Vicat softening point |
ASTM D-1525 |
105 |
ºC |
Flexural Modulus |
ASTM D-790 |
2007 |
Mpa |
APPLICATIONS: